National Graphite Announces Test Results

more »

Feyerabend directly oversaw the ultrasonic treatment of the sample material which yielded a dark gray powder with graphene characteristics. The field sample material was sieved to -60 mesh, five grams were weighed out and put into a clean Teflon beaker ...